Our company's carbon bipolar plates are the first carbon fiber reinforced flexible graphite bipolar plates in the industry. They do not break even when bent at 360°, with a compressive strength of ≥ 200 Mpa and a flexural strength of ≥ 50 Mpa. At a pressure of 0.2 Mpa, the hydrogen permeability is < 5 x 10-6 cm3/cm2·min. The electrical conductivity is > 30 S/cm. They can be applied in systems such as vanadium redox and zinc bromide.
| Name | Unit | Carbon fiber reinforced carbon-plastic bipolar plate |
| Thickness | mm | 0.6/0.8 |
| Density | g/cm³ | 1.4-1.6 |
| Width | mm | ≤900 |
| Length | mm | ≤1300 |
| Extension strength | Mpa | ≥50 |
| Compressive strength | Mpa | ≥100 |
| Conductivity in the conductive area | S/cm | ≥30 |
| Electrical conductivity in the welding area | S/cm | ≥30 |
| Carbon content | % | ≥60 |
| Hydrogen transmission rate(0.2Mpa) | cm3/cm2·min | <5x10-6 |
| Corrosion current | A | <5x10-6 |